google-site-verification=kQHsX0G5c-Leo6h-2qML__MlnH0_Sy9QpV_Lp5B4sHYgoogle-site-verification=favt3RhzayWvWaJ6ShEB5aT-wpo3L3QpCZAo4GtEOQU
google-site-verification=favt3RhzayWvWaJ6ShEB5aT-wpo3L3QpCZAo4GtEOQU
产品描述
材料:GS 93032-7-CR250Y440T-DP (1)
化学成分:
C% ≤ 0.14
Si% ≤ 0.50
Mn% ≤ 1.80
P% ≤ 0.080≦ 0.1
S% ≤ 0.015
AI% 0.015 bis/to 1.0
Ti+Nb% ≤ 0.15
Cr+Mo% ≤ 1.00
B% ≤ 0.005
力学性能:
YS 250 bis/to 330
TS(MPa) 440 bis/to 550
EL ≧27
材料:GS 93032-7-CR290Y490T-DP
化学成分:
C% ≤ 0.14
Si% ≤ 0.50
Mn% ≤ 1.80
P% ≤ 0.080≦ 0.1
S% ≤ 0.015
AI% 0.015 bis/to 1.0
Ti+Nb% ≤ 0.15
Cr+Mo% ≤ 1.00
B% ≤ 0.005
力学性能:
YS 290 bis/to 380
TS(MPa) 490 bis/to 600
EL ≧24
材料:GS 93032-7-CR330Y590T-DP
化学成分:
C% ≤ 0.15
Si% ≤ 0.75
Mn% ≤ 2.50
P% ≤ 0.040
S% ≤ 0.015
AI% 0.015 bis/to 1.5
Ti+Nb% ≤ 0.15
Cr+Mo% ≤ 1.40
B% ≤ 0.005
力学性能:
YS 330 bis/to 430
TS(MPa) 590 bis/to 700
EL ≧20
材料:GS 93032-7-CR440Y780T-DP
化学成分:
C% ≤ 0.18
Si% ≤ 0.80
Mn% ≤ 2.50
P% ≤ 0.080
S% ≤ 0.015
AI% 0.015 bis/to 2.0
Ti+Nb% ≤ 0.15
Cr+Mo% ≤ 1.40
B% ≤ 0.005
力学性能:
YS 440 bis/to 550
TS(MPa) 780 bis/to 900
EL ≧14
材料:GS 93032-7-CR700Y980T-DP
化学成分:
C% ≤ 0.23
Si% ≤ 1
Mn% ≤ 2.90
P% ≤ 0.080
S% ≤ 0.015
AI% 0.015 bis/to 2.0
Ti+Nb% ≤ 0.15
Cr+Mo% ≤ 1.40
B% ≤ 0.005
力学性能:
YS 700 bis/to 850
TS(MPa) 980 bis/to 1130
EL ≧8
材料:GS 93032-7-HR330Y580T-DP
化学成分:
C% ≤ 0.14
Si% ≤ 1
Mn% ≤ 2.20
P% ≤ 0.085
S% ≤ 0.015
AI% 0.015 bis/to 2.0
Ti+Nb% ≤ 0.15
Cr+Mo% ≤ 1.40
B% ≤ 0.005
力学性能:
YS 330 bis/to 450
TS(MPa) 580 bis/to 680
EL ≧19
使用范围:汽车、太阳能、金属制品、家用电器......
冷轧是通过冷压加工的热轧金属板的产品。由于多道次冷轧,冷轧板的表面质量优于热轧板,并且热处理后可以获得良好的力学性能。
根据生产企业的不同需求,冷轧板一般分为:冷轧钢板、冲压级冷轧钢板、深冲、超深冲和超深冲级冷轧钢板。
通常以卷和板的形式交付,厚度以mm表示,宽度一般为1000mm和1250mm,长度一般为2000mm和2500mm。